OK Aristorod 55

ESAB

OK Aristorod 55

The following items have been added to your list


x

OK AristoRod 55 is a 0.5Cr-0.5Ni-0.2Mo-alloyed, bare, solid wire for the GMAW of high strength steels. OK AristoRod 55 is treated with ESAB’s unique Advanced Surface Characteristics (ASC) technology, taking MAG welding operations to new levels of performance and all-round efficiency, especially in robotic and mechanised welding. Characteristic features include excellent start properties; trouble-free feeding at high wire speeds and lengthy feed distances; a very stable arc at high welding currents; extremely low levels of spatter; low fume emission; reduced contact tip wear and improved protection against corrosion of the wire.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded en 80ar/20co2 (m21)
75 J (56 ft-lb) -20 degC (-4 degF)
65 J (48 ft-lb) -30 degC (-22 degF)
60 J (44 ft-lb) -40 degC (-40 degF)
50 J (37 ft-lb) -50 degC (-58 degF)
50 J (37 ft-lb) -60 degC (-76 degF)
80 J (59 ft-lb) 0 degC (32 degF)
stress relieved en 80ar/20co2 (m21)
70 J (52 ft-lb) 1 hr 620 degC (1148 degF) -20 degC (-4 degF)
60 J (44 ft-lb) 1 hr 570 degC (1058 degF) -20 degC (-4 degF)
55 J (41 ft-lb) 1 hr 620 degC (1148 degF) -30 degC (-22 degF)
50 J (37 ft-lb) 1 hr 570 degC (1058 degF) -40 degC (-40 degF)
40 J (30 ft-lb) 1 hr 620 degC (1148 degF) -50 degC (-58 degF)
35 J (26 ft-lb) 1 hr 570 degC (1058 degF) -60 degC (-76 degF)
95 J (70 ft-lb) 1 hr 620 degC (1148 degF) 0 degC (32 degF)

Typical Tensile Properties

Condition As Welded Stress Relieved Stress Relieved
Shielding Gas EN 80Ar/20CO2 (M21) EN 80Ar/20CO2 (M21) EN 80Ar/20CO2 (M21)
Tensile Strength 770 MPa (112 ksi) 750 MPa (109 ksi) 750 MPa (109 ksi)
Yield Strength 690 MPa (100 ksi) 660 MPa (96 ksi) 660 MPa (96 ksi)
Elongation 20 % 24 % 24 %
Testing Time 1 hr 1 hr
Testing Temperature 620 degC (1148 degF) 570 degC (1058 degF)

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-280 A 1.0-5.4 kg/h (2-11 lb/h) 1.0 mm (0.040 in.) 18-28 V 2.7-14.7 m/min (106-579 in./min)
120-350 A 1.5-6.6 kg/h (3-14 lb/h) 1.2 mm (0.047 in.) 20-33 V 2.7-12.4 m/min (106-488 in./min)
225-480 A 3.3-11.6 kg/h (7-25 lb/h) 1.6 mm (1/16 in.) 26-38 V 3.5-12.0 m/min (138-472 in./min)
40-170 A 0.4-2.6 kg/h (0-5 lb/h) 0.8 mm (0.030 in.) 16-22 V 2.0-10.8 m/min (79-425 in./min)

Classifications

Classifications EN ISO 16834-A : G Mn3NiCrMo
EN ISO 16834-A : G 55 4 M Mn3NiCrMo
Wire Electrode SFA/AWS A5.28 : ER100S-G

Approvals

Approvals CE EN 13479
LR 4Y55S H5
NAKS/HAKC 1.2MM
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Low alloyed (0.5 % Cr, 0.5 % Ni, 0.2 % Mo)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo Ni P S Si
0.12 % 0.58 % - 1.38 % 0.20 % 0.53 % - - 0.71 %
Typical Weld Metal Analysis %
Ar/20CO2
0.11 % 0.5 % 0.07 % 1.1 % 0.2 % 0.5 % 0.015 % 0.015 % 0.5 %
x

Part Numbers and Accessories

Part Numbers : OK Aristorod 55
1B13086900 FIND A DISTRIBUTOR
1B13089300 FIND A DISTRIBUTOR
1B13106910 FIND A DISTRIBUTOR
1B13109320 FIND A DISTRIBUTOR
1B13122470 FIND A DISTRIBUTOR
1B13126910 FIND A DISTRIBUTOR
1B13129320 FIND A DISTRIBUTOR
1B13166910 FIND A DISTRIBUTOR
x
x

x

Loading..