OK Autrod 13.25 is a 1.0Ni-0.3Mo-0.1Ti-alloyed, copper-coated, solid wire for the GMAW of low-alloyed, high tensile strength steels and fine-grained steels for use in constructions such as bridges, offshore and hoists with a minimum yield strength of up to 610 MPa. The alloy has good impact properties down to -60°C. When used in mechanical pipe welding in narrow grooves, yield strengths in excess of 700 MPa may be obtained, permitting the overmatching of X80 pipeline steel.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded aws 80ar/20co2
90 J (67 ft-lb) -40 degC (-40 degF)
70 J (52 ft-lb) -60 degC (-76 degF)
140 J (104 ft-lb) 20 degC (68 degF)
as welded en 80ar/20co2
110 J (81 ft-lb) -40 degC (-40 degF)
70 J (52 ft-lb) -60 degC (-76 degF)
150 J (111 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

Condition As Welded As Welded
Shielding Gas AWS 80Ar/20CO2 EN 80Ar/20CO2
Tensile Strength 730 MPa (106 ksi) 740 MPa (107 ksi)
Yield Strength 640 MPa (93 ksi) 680 MPa (99 ksi)
Elongation 24 % 20 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-280 A 1.0-5.4 kg/h (2-11 lb/h) 1.0 mm (0.040 in.) 18-28 V 2.7-14.7 m/min (106-579 in./min)
120-350 A 1.5-6.6 kg/h (3-14 lb/h) 1.2 mm (0.047 in.) 20-33 V 2.7-12.4 m/min (106-488 in./min)

Classifications

Wire Electrode SFA/AWS A5.28 : ER100S-G
Weld Metal EN ISO 16834-A : G 62 6 M21 Mn3Ni1Mo
Wire Electrode EN ISO 16834-A : G Mn3Ni1Mo

Consumable Characteristics

Alloy Type Low alloyed (1 % Ni, 0.3 % Mo, 0.1 % Ti)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Mn Mo Ni P S Si Ti
0.08 % 1.70 % 0.38 % 0.95 % - - 0.60 % 0.08 %
Typical Weld Metal Analysis %
80Ar/20CO2 (M21)
0.07 % 1.5 % 0.3 % 0.95 % 0.01 % 0.01 % 0.5 % 0.05 %