Exaton 2209
2209 is used for welding of duplex stainless steels such as 2205 and 2304. It can also be used for welding of duplex stainless steels to carbon steel. It is used for TIG-welding.
Typical Charpy V-Notch Properties
as welded | ||||
Typical Tensile Properties
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 28 % | 710 MPa (103 ksi) | 580 MPa (84 ksi) |
Classifications
Wire Electrode |
SFA/AWS A5.9 : ER2209 EN ISO 14343-A : W 22 9 3 N L EN ISO 14343-B : 2209 |
Approvals
Approvals |
ABS ER 2209 BV ER 2209 CE EN 13479 DNV-GL Duplex Steels VdTÜV 19480 |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | Austenitic-ferritic (duplex) with approx. 55 FN ferrite - 22.5% Cr - 8% Ni - 3% Mo - Low C |
Shielding Gas | I1, I2, I3, N2 (EN ISO 14175) |
Typical Weld Metal Analysis %
Typical Weld Metal Analysis % | ||||||||||||||||
C | Co | Cr | Cu | FN WRC-92 | Mn | Mo | N | Nb | Ni | P | PRE | S | Si | Ti | V | W |
0.01 % | - | 23 % | 0.1 % | 54 % | 1.5 % | 3.1 % | 0.16 % | 0.01 % | 8.5 % | 0.02 % | 35.8 % | 0.001 % | 0.5 % | - | - | 0.01 % |
Typical Wire Composition % | ||||||||||||||||
0.012 % | 0.04 % | 23 % | 0.09 % | 55 % | 1.5 % | 3.2 % | 0.15 % | 0.01 % | 8.6 % | 0.018 % | 37 % | 0.0007 % | 0.5 % | 0.003 % | 0.05 % | 0.01 % |